This course is designed to provide a practical understanding of fractography through a combination of lecture and hands on experience. Theory and examples presented in the lectures are reinforced by macro and micro examination of failed parts in the lab.
|
|
| |
|
|
|
|
| |
|
|
Course Coverage |
|
| |
|
|
|
|
| |
|
|
Visual examination as well as stereo microscopy and scanning electron microscopy will be utilized to interpret example fractures. Improve your skills in this vital portion of most failure examinations. |
|
| |
|
|
|
|
| |
|
|
Course Details
|
|
| |
|
|
|
|
| |
|
|
Dates: |
Date to be advised
|
|
| |
|
|
Time: |
9am - 5pm |
|
| |
|
|
Venue: |
IMR Test Labs - Singapore
30 Loyang Way #03-16
Singapore 508769
|
|
| |
|
|
Fees: |
Public: S$1,995/pax (excl. prevailing GST)
ATVs Category: CAT B
AAIS Members: make use of your ATVs !
|
|
| |
|
|
Register: |
Email registration form to training@aais.org.sg |
|
| |
|
|
Closing Date: |
One week before course date.
*Note: Class commencement is subject to minimum class size requirements.
|
|
| |
|
|
|
|
|
| |
|
|
About the Instructor
|
|
| |
|
|
Mr Ronald J. Parrington, P.E., FASM, President of IMR Test Labs
|
|
| |
|
|
Ron is a graduate of Rensselaer Polytechnic Institute with BS and MS degrees in materials engineering. He has over 30 years of experience in testing and failure analysis of metallic and nonmetallic materials. He has presented and published numerous papers on failure analysis and teaches the courses Principles of Failure Analysis, Practical Fractography, and Introduction to Polymers and Polymer Testing. He previously served as chairman of the ASM International Failure Analysis Committee and currently serves as the chairman of the ASM Materials Education Foundation Board of Trustees.
About IMR Test Labs
IMR Test Labs is an international firm offering a complete scope of materials testing services, including chemical analysis, mechanical testing, metallurgical analysis, failure analysis, fatigue testing, training and much more.
With four state-of-the-art facilities, located in Ithaca, New York; Louisville, Kentucky; Portland, Oregon and Singapore. IMR Test Labs will be expanding into China with a new facility opening in the Suzhou industrial park in August of 2012.
IMR Test Labs materials testing labs are accredited by A2LA (NY, KY & OR), Nadcap (NY, OR), SAC (SPR), GE S-400 (NY, KY, OR & SPR) and many major manufacturers around the world.
Behind the doors of IMR Test Labs' facilities are over 130 knowledgeable, experienced professionals — PhDs, engineers, chemists, metallurgists, technicians and support staff — who work side by side with clients in a diverse range of industries.
About ASM International
ASM International serves materials professionals, non-technical personnel, and managers worldwide by providing high-quality materials information, education and training, networking opportunities, and professional development resources in cost-effective and user-friendly formats.
As an engineering and scientific society, ASM represents over 34,000 members residing in over 100 different countries worldwide. These members represent a broad industry base contributing to advances in materials for aerospace, automotive, electronics and medical device industries to name a few. Established in 1913, ASM has nearly 100 years of experience in connecting the materials community to resources that allow them to solve problems quickly, identify opportunities for business development and improve the quality of life for the entire world.
|
|
| |
|
|
|
 |  |
A warm welcome to our newest members!
Agnos Chemicals Pte Ltd
Ametek Singapore Pte Ltd
CNC Design Pte Ltd
Sunway E-Systems (Singapore) Pte Ltd
Wencor, LLC
| |
AAIS Extraordinary General Meeting
concluded on 3rd May 2012
4pm @ the AAIS Boardroom
The AAIS General Assembly elects
MR TIN HO
Rolls-Royce Singapore Pte Ltd
as 2nd Vice President for
the current term of office.
WE HAVE MOVED!
Please note our new address:
4 Changi South Lane
#07-01A, AAIS AeroHub
Nan Wah Building
Singapore 486127
|
| |
|
Apr-Jun 2012 issue out now!
Grab your copy today!
Click here to subscribe
|

|